The AlSi10Mg alloy was processed by selective laser melting using both hot-and cold-build platforms. The investigation was aimed at defining suitable platform pre-heating and post-process thermal treatment strategies, taking into consideration the peculiar microstructures generated. Microstructural analyses, differential scanning calorimetry, and high-resolution diffraction from synchrotron radiation, showed that in the cold platform as-built condition, the amount of supersaturated Si was higher than in hot platform samples. The best hardness and tensile performance were achieved upon direct aging from cold platform-printed alloys. The hot platform strategy led to a loss in the aging response, since the long processing times spent at high temperature induced a substantial overaging effect, already in the as-built samples. Finally, the standard T6 temper consisting of post-process solution annealing followed by artificial aging, resulted in higher ductility but lower mechanical strength.

Effects of platform pre-heating and thermal-treatment strategies on properties of alsi10mg alloy processed by selective laser melting

Coduri M.;
2018-01-01

Abstract

The AlSi10Mg alloy was processed by selective laser melting using both hot-and cold-build platforms. The investigation was aimed at defining suitable platform pre-heating and post-process thermal treatment strategies, taking into consideration the peculiar microstructures generated. Microstructural analyses, differential scanning calorimetry, and high-resolution diffraction from synchrotron radiation, showed that in the cold platform as-built condition, the amount of supersaturated Si was higher than in hot platform samples. The best hardness and tensile performance were achieved upon direct aging from cold platform-printed alloys. The hot platform strategy led to a loss in the aging response, since the long processing times spent at high temperature induced a substantial overaging effect, already in the as-built samples. Finally, the standard T6 temper consisting of post-process solution annealing followed by artificial aging, resulted in higher ductility but lower mechanical strength.
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11571/1370575
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 129
  • ???jsp.display-item.citation.isi??? ND
social impact