Crystal shape control on a series of anatase photocatalysts was achieved by varying the amount of HF employed as a capping agent in their hydrothermal synthesis. A systematic comparison between their physicochemical properties, determined by several complementary surface and bulk techniques before and after thermal treatment at 500 °C, allowed one to discern the influence of the relative amount of exposed {001} crystal facets among a series of effects simultaneously affecting their oxidative photocatalytic activity. The results of both formic acid and terephthalic acid photo-oxidation test reactions point to the primary role played by calcination in making {001} facets effectively photoactive. Annealing not only removes most of the residual fluorine capping agent from the photocatalyst surface, thus favoring substrate adsorption, but also produces morphological modifications to a crystal packing that makes accessible a larger portion of surface {001} facets due to the unpiling of platelike crystals. The photocatalyst bearing the highest amount of exposed {001} facets (60%) shows the highest photoactivity in both the direct and the •OH-radical-mediated photocatalytic test reaction.

Unraveling the Multiple Effects Originating the Increased Oxidative Photoactivity of {001}-Facet Enriched Anatase TiO2

Coduri M.;
2016-01-01

Abstract

Crystal shape control on a series of anatase photocatalysts was achieved by varying the amount of HF employed as a capping agent in their hydrothermal synthesis. A systematic comparison between their physicochemical properties, determined by several complementary surface and bulk techniques before and after thermal treatment at 500 °C, allowed one to discern the influence of the relative amount of exposed {001} crystal facets among a series of effects simultaneously affecting their oxidative photocatalytic activity. The results of both formic acid and terephthalic acid photo-oxidation test reactions point to the primary role played by calcination in making {001} facets effectively photoactive. Annealing not only removes most of the residual fluorine capping agent from the photocatalyst surface, thus favoring substrate adsorption, but also produces morphological modifications to a crystal packing that makes accessible a larger portion of surface {001} facets due to the unpiling of platelike crystals. The photocatalyst bearing the highest amount of exposed {001} facets (60%) shows the highest photoactivity in both the direct and the •OH-radical-mediated photocatalytic test reaction.
2016
Inglese
8
15
9745
9754
10
•; OH radicals; anatase {001} facets; holes; photocatalysis; photocatalytic oxidation; surface fluorination
no
6
info:eu-repo/semantics/article
262
Maisano, M.; Dozzi, M. V.; Coduri, M.; Artiglia, L.; Granozzi, G.; Selli, E.
1 Contributo su Rivista::1.1 Articolo in rivista
none
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11571/1466325
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 47
  • ???jsp.display-item.citation.isi??? ND
social impact