A Nd:BLG disordered crystal was passively mode-locked. We obtained 316-fs long pulses at 1060 nm and sub-ps pulses on a wide, continuous tuning range extending from 1072 nm to 1090 nm.

Widely Tunable Femtosecond Pulses Generated by a Nd3+:BaLaGa3O7 Disordered Crystal

AGNESI, ANTONIANGELO;PIRZIO, FEDERICO;TARTARA, LUCA;UGOLOTTI, ELENA;
2013-01-01

Abstract

A Nd:BLG disordered crystal was passively mode-locked. We obtained 316-fs long pulses at 1060 nm and sub-ps pulses on a wide, continuous tuning range extending from 1072 nm to 1090 nm.