Skeletal muscle tissue engineering holds immense promise for volumetric muscle loss treatment and in vitro disease modelling. However, fabricating functional, highly organized muscle constructs remains a challenge [1,2]. In this context, a particularly promising field is the combination of different scaffolds (such as hydrogels), to create three-dimensional structures that mimic the complex architecture of native muscle. This study investigates the use of dif-ferent hydrogels provided by CELLINK® combined with a murine myoblast cell line (C2C12) to evaluate the syner-gistic effects on cellular viability and myogenic maturation. C2C12 cells were encapsulated into three distinct hydro-gel formulations —GelXA Fibrin + CACl2, CELLINK GelMA, CELLINK GelMA + CACl2—seeded on different scaffolds and analysed morphologically at 24 hour and days 1, and 7 utilizing a Live/Dead cell staining assay. Fol-lowing the preliminary ink screening phase, the fibrinogen-based hydrogel from CELLINK® was selected as the gold standard for printing muscle cells. Our next step was to combine the constructs with stretchable scaffolds, enabling the use of a bioreactor to simulate muscle mechanical contraction. We used PDMS (Polydimethylsiloxane) as a high-ly versatile silicone elastomer widely utilized in muscle tissue engineering (SMTE), not only because its biological compatibility, but also because of its mechanical properties [3]. To optimize the cell-scaffold interface, the PDMS supports were conditioned with two different coatings: collagen and Matrigel. The latter is a solubilized extracellular matrix derived from the Engelbreth-Holm-Swarm (EHS) mouse sarcoma, used to promote cell adhesion. C2C12 cells were seeded onto these conditioned supports, the resulting constructs were maintained in culture for a period of 1 week to evaluate viability and muscle differentiation, using morphological and qRT-PCR analyses, at days 3 and 7 of culture. A Live/Dead kit and phalloidin staining, a highly selective marker for actin filaments were used. The results on the "collagen-coated" samples revealed significant technical criticalities, as high autofluorescence was observed, which masked the signal emitted by the fluorescent probes. In contrast, the Matrigel-conditioned samples allowed a clear visualization of the cells seeded on the muscle constructs as early as 3 days of culture, confirming the presence of viable and elongated cells within the construct. Molecular biology analysis conducted at 7 days compared the tran-scriptional profile of C2C12 cells seeded on PDMS-Matrigel constructs with respect to control cells seeded on plastic (2D). The results showed that the Myoferlin, Myosin, and Myomaker genes exhibited a statistically significant higher expression in 2D samples compared to the constructs, indicating that the myogenic differentiation process in PDMS/hydrogel samples is still delayed. Consequently, the 3D differentiation protocol requires further optimization. Future analysis will focus on modulating conditioning parameters and introducing mechanical stimulation using the bioreactor, in order to promote proper myogenesis in the 3D constructs.
Development of Skeletal Muscle Analogues via Optimization of Different Hydrogels and Scaffolds
LAURA BENEDETTI;MATTEO BENTIVEGNA;FRANCA SCOCOZZA;MICHELE CONTI;MARIAROSA POLIMENI;RENATA BORATTO;GABRIELLA CUSELLA;GABRIELE CECCARELLI
Writing – Review & Editing
2026-01-01
Abstract
Skeletal muscle tissue engineering holds immense promise for volumetric muscle loss treatment and in vitro disease modelling. However, fabricating functional, highly organized muscle constructs remains a challenge [1,2]. In this context, a particularly promising field is the combination of different scaffolds (such as hydrogels), to create three-dimensional structures that mimic the complex architecture of native muscle. This study investigates the use of dif-ferent hydrogels provided by CELLINK® combined with a murine myoblast cell line (C2C12) to evaluate the syner-gistic effects on cellular viability and myogenic maturation. C2C12 cells were encapsulated into three distinct hydro-gel formulations —GelXA Fibrin + CACl2, CELLINK GelMA, CELLINK GelMA + CACl2—seeded on different scaffolds and analysed morphologically at 24 hour and days 1, and 7 utilizing a Live/Dead cell staining assay. Fol-lowing the preliminary ink screening phase, the fibrinogen-based hydrogel from CELLINK® was selected as the gold standard for printing muscle cells. Our next step was to combine the constructs with stretchable scaffolds, enabling the use of a bioreactor to simulate muscle mechanical contraction. We used PDMS (Polydimethylsiloxane) as a high-ly versatile silicone elastomer widely utilized in muscle tissue engineering (SMTE), not only because its biological compatibility, but also because of its mechanical properties [3]. To optimize the cell-scaffold interface, the PDMS supports were conditioned with two different coatings: collagen and Matrigel. The latter is a solubilized extracellular matrix derived from the Engelbreth-Holm-Swarm (EHS) mouse sarcoma, used to promote cell adhesion. C2C12 cells were seeded onto these conditioned supports, the resulting constructs were maintained in culture for a period of 1 week to evaluate viability and muscle differentiation, using morphological and qRT-PCR analyses, at days 3 and 7 of culture. A Live/Dead kit and phalloidin staining, a highly selective marker for actin filaments were used. The results on the "collagen-coated" samples revealed significant technical criticalities, as high autofluorescence was observed, which masked the signal emitted by the fluorescent probes. In contrast, the Matrigel-conditioned samples allowed a clear visualization of the cells seeded on the muscle constructs as early as 3 days of culture, confirming the presence of viable and elongated cells within the construct. Molecular biology analysis conducted at 7 days compared the tran-scriptional profile of C2C12 cells seeded on PDMS-Matrigel constructs with respect to control cells seeded on plastic (2D). The results showed that the Myoferlin, Myosin, and Myomaker genes exhibited a statistically significant higher expression in 2D samples compared to the constructs, indicating that the myogenic differentiation process in PDMS/hydrogel samples is still delayed. Consequently, the 3D differentiation protocol requires further optimization. Future analysis will focus on modulating conditioning parameters and introducing mechanical stimulation using the bioreactor, in order to promote proper myogenesis in the 3D constructs.I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.